Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 77.2 - 234 MPa | 11200 - 34000 psi | Average value: 175 MPa Grade Count:12 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Tensile Strength, Ultimate | 77.2 MPa | 11200 psi | |
BCC Products BC 5003 Epoxy Laminating System BC 5003 is a medium viscosity, unfilled laminating system. It is a room temperature curing resin with a relatively short pot life. BC 5003 is also considered an excellent general purpose adhesive fo.. |