Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 74.5 MPa | 10800 psi | ASTM D638 |
Nylene® 6111 (HS) , 40% Glass/Mineral Reinforced Nylon 6/6 Description: Nylene® 6111 (HS) is a 40% mineral reinforced, impact modified nylon 6/6. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Pol.. |
|||
Tensile Strength, Ultimate | 74.5 MPa | 10800 psi | |
Hybrid Plastics Nanoreinforced® POSS® 5% POSS-polyimide Nanoreinforced® POSS® Polyimide is a hybrid nanocomposite that can serve as oxidation resistant and highly bondable form of polyimide. Upon exposure to oxidizing oxygen the POSS® polyimide .. |