Material Notes:
Description: Nylene® 6111 (HS) is a 40% mineral reinforced, impact modified nylon 6/6. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 74.5 MPa
10800 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 235 °C
455 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
ASTM D648
Users viewing this material also viewed the following: