Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 73.77 MPa
10700 psi
Abatron AboCast 8-12/Abocure 8-12 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/13.2 ratio (pbw); Gel time, 100 g (3.5 oz.): 49 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F..