Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.80 MPa | 1130 psi | ISO 37 |
Multibase TPSiV® 4200-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Tensile Strength, Ultimate | 7.80 MPa | 1130 psi | GB/T 528 |
Chengdu Polyster FR2085 Flame Retardant Grade TPV Good heat stability and light stability. Meets the requirements of European Dioxine Principle and the environmental protection criteria. Can be used for wires, cables, buncles, carcass of train.Inf.. |