Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 46.2 MPa | 6700 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 46.2 MPa | 6700 psi | |
Kraton® G1657 + PA-6,6 blend (16/4/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Tensile Strength, Ultimate | 46.2 MPa | 6700 psi | |
Elastomer Engineering E95C Polyurethane A high-performance, moderate cost formulation. A polyester/ether that combines many of the best properties of both polyester-based and polyether-based elastomers. Typical uses: Wheels, rolls, pist.. |
|||
Tensile Strength, Ultimate | 46.2 MPa | 6700 psi | ASTM Data |
Americas Styrenics Styron® 612 Polystyrene
(discontinued **) STYRON® 612 general purpose polystyrene resin is an easy flow resin with no color additives. When used unmodified for the manufacture of food contact articles STYRON 612 complies with the US Food, .. |