Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 46.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 46.2 MPa
6700 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated  (discont
Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 46.2 MPa
6700 psi
Kraton® G1657 + PA-6,6 blend (16/4/80)
Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..
Tensile Strength, Ultimate 46.2 MPa
6700 psi
Elastomer Engineering E95C Polyurethane
A high-performance, moderate cost formulation. A polyester/ether that combines many of the best properties of both polyester-based and polyether-based elastomers. Typical uses: Wheels, rolls, pist..
Tensile Strength, Ultimate 46.2 MPa
6700 psi
ASTM Data
Americas Styrenics Styron® 612 Polystyrene  (discontinued **)
STYRON® 612 general purpose polystyrene resin is an easy flow resin with no color additives. When used unmodified for the manufacture of food contact articles STYRON 612 complies with the US Food, ..