Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 410 MPa @Temperature 100 °C |
59500 psi @Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Ultimate | 410 MPa @Temperature 100 °C |
59500 psi @Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Ultimate | 410 MPa @Temperature 300 °C |
59500 psi @Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Ultimate | 410 MPa @Temperature 300 °C |
59500 psi @Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Ultimate | 410 MPa @Temperature 300 °C |
59500 psi @Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Ultimate | 410 MPa @Temperature 300 °C |
59500 psi @Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Ultimate | 410 MPa @Temperature 300 °C |
59500 psi @Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Tensile Strength, Ultimate | 410 - 590 MPa | 59500 - 85600 psi | |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; A (TB00) Temper (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 410 - 590 MPa | 59500 - 85600 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 410 - 590 MPa | 59500 - 85600 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 410 - 590 MPa | 59500 - 85600 psi | |
Materion Beryllium Copper Alloy 25 Forgings & Extrusions; A (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 410 - 590 MPa | 59500 - 85600 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 410 - 590 MPa | 59500 - 85600 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 410 - 530 MPa | 59500 - 76900 psi | |
Materion Beryllium Copper Alloy 25 Strip; A -Dead Soft (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Tensile Strength, Ultimate | 410 - 540 MPa | 59500 - 78300 psi | |
Materion Beryllium Copper Alloy 25 Strip; A -Planished (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Tensile Strength, Ultimate | 410 - 590 MPa | 59500 - 85600 psi | |
Materion Beryllium Copper Alloy 25 Tube; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 410 - 590 MPa | 59500 - 85600 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 410 - 510 MPa | 59500 - 74000 psi | |
SSAB Tunnplat Docol® 350YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Tensile Strength, Ultimate | 410 - 460 MPa | 59500 - 66700 psi | |
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Tensile Strength, Ultimate | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 1011, Grade 45 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Tensile Strength, Ultimate | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 607 Class 2 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Ultimate | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 715 Class 2 Formable, Grade 50F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Ultimate | >= 410 MPa | >= 59500 psi | |
AK Steel CL 2/ SAE J1392 045 XLK, Grade 50 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 410 MPa | >= 59500 psi | |
AK Steel ASTM A 570, Grade 45 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |