Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 410 - 530 MPa | 59500 - 76900 psi | |
Materion Beryllium Copper Alloy 25 Strip; A -Dead Soft (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Tensile Strength, Ultimate | 490 - 530 MPa | 71100 - 76900 psi | T direction |
ArcelorMittal Torque 20-15 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 490 - 530 MPa | 71100 - 76900 psi | T direction |
ArcelorMittal Torque 25-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 490 - 530 MPa | 71100 - 76900 psi | T direction |
ArcelorMittal Torque 27-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 490 - 530 MPa | 71100 - 76900 psi | T direction |
ArcelorMittal Torque 30-17 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 490 - 530 MPa | 71100 - 76900 psi | T direction |
ArcelorMittal Torque 30-18 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Ultimate | 450 - 530 MPa | 65300 - 76900 psi | |
ArcelorMittal Dual Phase 450 Very high strength steel, Cold Rolled Steel Available in the following: HCT500X (uncoated), HCT500X+ZE (electrogalvanized) and HCT500X+Z (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength and .. |
|||
Tensile Strength, Ultimate | 460 - 530 MPa | 66700 - 76900 psi | |
ArcelorMittal HSLA 380 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC380LA), electroglavanized (HC380LA +ZE) and Extragal®/galfan/Galvannealed (HC380LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |