Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 593 MPa | 86000 psi | |
Universal Wire Works 308L Stainless Steel Electrode Universal 308L is the low carbon version of 308 and is designed for welding 304L stainless steel. The weld deposit contains a maximum of 0.04 carbon which minimizes the formation of chromium carbide.. |
|||
Tensile Strength, Ultimate | 593 MPa | 86000 psi | |
Universal Wire Works 316L Stainless Steel Electrode Universal 316L is the same as Alloy 316 except for the restricted carbon content. By holding the carbon content below 0.04% the chances of carbon precipitation is minimized thus protecting the corro.. |
|||
Tensile Strength, Ultimate | 593 MPa @Temperature 93.0 °C |
86000 psi @Temperature 199 °F |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Ultimate | 593 MPa | 86000 psi | Annealed, Fine blanking quality |
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Ultimate | 593 MPa @Temperature 260 °C |
86000 psi @Temperature 500 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Ultimate | 593 - 676 MPa | 86000 - 98000 psi | |
Eagle Brass 752 Nickel Silver 18%, Extra Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |