Universal Wire Works 316L Stainless Steel Electrode

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 316L Stainless Steel Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 316L is the same as Alloy 316 except for the restricted carbon content. By holding the carbon content below 0.04% the chances of carbon precipitation is minimized thus protecting the corrosion resistance of the base metal. Universal 316L is used extensively in the chemical and process industries and on parts and equipment build to resist acids used in the manufacture of ink, paints, rubber, synthesized fabrics, bleaches, photographic chemicals and pulp and paper.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 593 MPa
86000 psi
Elongation at Break 42 %
42 %
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Chromium, Cr 18.5 %
18.5 %
Iron, Fe 64.1 %
64.1 %
As Remainder
Manganese, Mn 1.75 %
1.75 %
Molybdenum, Mo 2.25 %
2.25 %
Nickel, Ni 12.9 %
12.9 %
Silicon, Si 0.50 %
0.50 %