Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4000 MPa
580000 psi
Toho Tenax Besfight® STS 24K HTA-7C F301 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..
Tensile Strength, Ultimate 4000 MPa
580000 psi
China Tungsten YG12X Tungsten Carbide
Information provided by China Tungsten