Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 4000 MPa | 580000 psi | |
Toho Tenax Besfight® STS 24K HTA-7C F301 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Tensile Strength, Ultimate | 4000 MPa | 580000 psi | |
China Tungsten YG12X Tungsten Carbide Information provided by China Tungsten |