Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 395 MPa | 57300 psi | Typical |
Aleris Weldural Aluminum Alloy, 600 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |
|||
Tensile Strength, Ultimate | 395 MPa | 57300 psi | Typical |
Aleris Weldural Aluminum Alloy, 700 mm Thickness Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab.. |