Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 56.5 MPa | 8200 psi | TM R050-36 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Tensile Strength, Ultimate | 56.5 MPa | 8200 psi | TM R050-36 |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Tensile Strength, Ultimate | 56.5 MPa | 8200 psi | ASTM D412 |
2095A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 56.5 MPa | 8200 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AS-20GF/05T Acrylonitrile Butadiene Styrene (ABS), Glass Filled, PTFE Lubricated
(discont Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 56.5 MPa | 8200 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-20GF-05GB/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 56.5 MPa @Thickness 3.17 mm |
8190 psi @Thickness 0.125 in |
ASTM D638 |
LG Chemical Lupox® PBT-GP-1000 High Flow PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 56.5 MPa | 8200 psi | ASTM D412 |
Lubrizol Estane® ALR E95A Thermoplastic Polyurethane Type: Estane® ALR E95A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |
|||
Tensile Strength, Ultimate | 56.5 MPa | 8190 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ ES-5500C TC-EM Polyethersulfone
(discontinued **) Description/Features:Thermally ConductiveCeramic FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |