Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 97
97
ASTM D2240
Tensile Strength, Ultimate 56.5 MPa
8200 psi
ASTM D412
Tensile Strength, Yield 11.0 MPa
1600 psi
at 100%; ASTM D412
Elongation at Break 450 %
450 %
ASTM D412