Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 551 MPa | 79900 psi | |
Kennametal Stellite Stellite® 250 Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.Applications:heat treatment furnace.. |
|||
Tensile Strength, Ultimate | 551 - 620 MPa | 79900 - 89900 psi | |
Ametek AM 388™ Alloy (UNS C72650) TD03 3/4 Hard Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Ultimate | 551 MPa | 79900 psi | |
ATI Allvac® Nickelvac® 400 UNS N04400 Nickel Superalloy Nickel-Copper solid solution alloy. Uses: Equipment for mineral acids, brines, alkalis, offshore engineering, marine applications.Property values are for samples in the metallurgical condition: 165.. |
|||
Tensile Strength, Ultimate | 551 MPa | 79900 psi | |
ATI Allvac® Nickelvac® 825 UNS N08825 Nickel Superalloy Uses: Downhole tubulars for deep, corrosive wells. Pollution control, scrubber, and radwaste systems. CPI process piping systems.Property values are for samples in the metallurgical condition: 2100°.. |
|||
Tensile Strength, Ultimate | 551 MPa | 79900 psi | Longitudinal, Welded |
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406 Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat.. |