ATI Allvac® Nickelvac® 825 UNS N08825 Nickel Superalloy

Category Metal , Superalloy , Iron Base
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® 825 UNS N08825 Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: Downhole tubulars for deep, corrosive wells. Pollution control, scrubber, and radwaste systems. CPI process piping systems.Property values are for samples in the metallurgical condition: 2100°C anneal.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.13 g/cc
0.294 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Tensile Strength, Ultimate 551 MPa
79900 psi
Tensile Strength, Yield 186 MPa

@Strain 0.200 %
27000 psi

@Strain 0.200 %
Elongation at Break 40 %
40 %
Reduction of Area 70 %
70 %
Component Elements Properties Metric English Comments
Aluminum, Al 0.10 %
0.10 %
Carbon, C 0.020 %
0.020 %
Chromium, Cr 21.5 %
21.5 %
Copper, Cu 2.2 %
2.2 %
Iron, Fe 30 %
30 %
as balance
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 3.0 %
3.0 %
Nickel, Ni 42 %
42 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.010 %
0.010 %
Titanium, Ti 0.90 %
0.90 %