Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 - 55.8 MPa
2900 - 8100 psi
Average value: 42.6 MPa Grade Count:74
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..