Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 55.1 MPa | 7990 psi | ASTM D638-03 |
Objet FullCure® 840 Vero Blue Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Tensile Strength, Ultimate | 55.1 MPa @Temperature 110 °C |
7990 psi @Temperature 230 °F |
ASTM D638 |
Saint-Gobain Meldin® 7021 Direct Formed Graphite Filled Polyimide Finished parts and basic shapes made from 15% by weight graphite filled polyimide material for applications high wear resistance, good thermal oxidative stability, and high temperature resistance. .. |