Material Notes:
Information provided by American Precision Prototyping, LLC
Physical Properties Metric English Comments
Water Absorption at Saturation 1.87 %
1.87 %
ASTM D570-98
Ash <= 0.30 %
<= 0.30 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 81
81
Hardness, Shore D 83
83
Tensile Strength, Ultimate 55.1 MPa
7990 psi
ASTM D638-03
Elongation at Break 20 %
20 %
ASTM D412
Tensile Modulus 2.74 GPa
397 ksi
ASTM D638-04
Flexural Strength 83.6 MPa
12100 psi
ASTM D790-03
Flexural Modulus 1.983 GPa
287.6 ksi
ASTM D790-04
Izod Impact, Notched 0.236 J/cm
0.442 ft-lb/in
ASTM D256-06
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 48.8 °C
120 °F
ASTM D648-06
Deflection Temperature at 1.8 MPa (264 psi) 44.8 °C
113 °F
ASTM D648-06
Glass Transition Temp, Tg 48.7 °C
120 °F
DMA, E"
Users viewing this material also viewed the following: