Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.5 - 52.5 MPa @Temperature 130 - 175 °C |
3990 - 7610 psi @Temperature 266 - 347 °F |
Average value: 70.7 MPa Grade Count:2 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Tensile Strength, Ultimate | 27.5 - 52.5 MPa @Time 1.80e+7 - 7.20e+7 sec |
3990 - 7610 psi @Time 5000 - 20000 hour |
Average value: 70.7 MPa Grade Count:2 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |