Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.4 MPa
7450 psi
ASTM D638
Multibase Nylex™ 4032 Black Polyamide + PP
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tensile Strength, Ultimate 51.4 MPa
7450 psi
BCC Products BC 6128 Epoxy, Hi-Heat, Abrasion Resistant
BC 6128 is a black, non-staining, silicon carbide filled, “die surface” surfacing resin. This thixotropic resin system provides excellent surface duplication along with good vertical coverage. Ext..