Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 50.4 MPa | 7310 psi | ASTM Data |
Styron Pulse® 959 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 959 Engineering resin is a 10% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 959 Engineering resin has been used.. |