Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5.49 MPa | 797 psi | |
Momentive Performance Materials RTV167 Electronic Grade Silicone Adhesive Sealant, Gray RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Tensile Strength, Ultimate | 5.49 MPa | 796 psi | |
Momentive Performance Materials RTV167 Gray Adhesive Sealant, Non-Corrosive High Strength One-part totally non-corrosive alkoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: Highest strength ad.. |
|||
Tensile Strength, Ultimate | 5.49 MPa | 797 psi | |
Momentive Performance Materials RTV566 Silicone Rubber Compound for Low Outgassing Applications RTV566 silicone rubber compound is a two-part product processed and tested for applications where low outgassing is required. RTV566A base compound is supplied ready to use with RTV566B curing agen.. |
|||
Tensile Strength, Ultimate | 5.49 MPa | 796 psi | |
Momentive Performance Materials RTV566 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Tensile Strength, Ultimate | 5.49 MPa @Treatment Temp. 150 °C, Time 605000 sec |
797 psi @Treatment Temp. 302 °F, Time 168 hour |
Heat Aging; ASTM D 412/ASTM D 573 |
Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate Neoplast 155 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, .. |
|||
Tensile Strength, Ultimate | 5.49 MPa @Treatment Temp. 150 °C, Time 605000 sec |
797 psi @Treatment Temp. 302 °F, Time 168 hour |
Heat Aging; ASTM D 412/ASTM D 573 |
Zylog Neoplast® 155 FT SWB Thermoplastic Vulcanizate Neoplast 155 FT SWB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant,.. |