Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 5.10 MPa | 740 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO D 3218 Multi-Flex® TPO D 3218 is a compound for automotive applications replacing Himont's 7023. The burn rate is 0.6 in/min; ASTM FM VSS 30.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 5.10 MPa | 740 psi | ASTM D638 |
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 59 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e.. |
|||
Tensile Strength, Ultimate | 5.10 MPa | 740 psi | ASTM D638 |
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 58 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e.. |
|||
Tensile Strength, Ultimate | 5.10 MPa | 740 psi | JIS K6301 |
Stellarchem AB870EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Tensile Strength, Ultimate | 5.10 MPa | 740 psi | JIS K6301 |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |