Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.43 MPa | 498 psi | |
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive TSE326 is a one-component, heat curing silicone adhesive which offers extended performance at temperatures exceeding 200C. A flowable material with primerless adhesion to many substrates, it is suit.. |