Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 3.43 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.43 MPa
498 psi
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive
TSE326 is a one-component, heat curing silicone adhesive which offers extended performance at temperatures exceeding 200C. A flowable material with primerless adhesion to many substrates, it is suit..
Tensile Strength, Ultimate 3.43 MPa
497 psi
Momentive Performance Materials TSE326 Red Adhesive Sealant, Non-Corrosive Flowable High Temperature
One-part heat cure. Typical uses: Assembly and gasketing.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.