Polymer Property : Tensile Strength, Ultimate = 49700.1 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 - 342.669 MPa

@Temperature -40.0 - 150 °C
9430 - 49700.1 psi

@Temperature -40.0 - 302 °F
Average value: 128 MPa Grade Count:9
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..