Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 484 MPa @Temperature 816 °C |
70200 psi @Temperature 1500 °F |
|
Kennametal Stellite Stellite® 6K 1.6 mm thick sheet 13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, g.. |
|||
Tensile Strength, Ultimate | 484 MPa @Temperature 538 °C |
70200 psi @Temperature 1000 °F |
ASTM E8 |
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 484 MPa | 70200 psi | 5% Cold Worked |
AK Steel 439 ULTRA FORM® Stainless Steel AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul.. |