Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.04 MPa | 441 psi | |
Momentive Performance Materials RTV577 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Tensile Strength, Ultimate | 3.04 MPa | 441 psi | |
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Tensile Strength, Ultimate | 3.04 MPa | 441 psi | JIS K6301 |
Stellarchem DIOSHY® GP-935-UB2 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Tensile Strength, Ultimate | 3.04 MPa | 441 psi | JIS K6301 |
Stellarchem LP-880 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |