Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone, RTV, Encapsulation Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough materials, highly resistant to contamination, and will not be affected by other chemicals during cure or after. Typical uses: Aerospace sealing and insulating; vertical and overhead surfaces.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Viscosity 700000 cP

@Temperature 25.0 °C
700000 cP

@Temperature 77.0 °F
Linear Mold Shrinkage 0.0065 cm/cm
0.0065 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
Tensile Strength, Ultimate 3.04 MPa
441 psi
Elongation at Break 120 %
120 %
Tear Strength 6.80 kN/m
38.8 pli
Die B
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.310 W/m-K
2.15 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
399 °F
Continuous useful temperature.
Minimum Service Temperature, Air -115 °C
-175 °F
Continuous useful temperature.
Electrical Properties Metric English Comments
Electrical Resistivity 5.60e+14 ohm-cm
5.60e+14 ohm-cm
Dielectric Constant 3.98

@Frequency 1000 Hz
3.98

@Frequency 1000 Hz
Dielectric Strength 18.5 kV/mm

@Thickness 1.91 mm
470 kV/in

@Thickness 0.0750 in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Cure time 24 hrs.
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
Copyright © lookpolymers.com All Rights Reserved