Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 380 MPa @Temperature 400 °C |
55100 psi @Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Ultimate | 380 MPa @Temperature 300 °C |
55100 psi @Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Ultimate | 380 MPa @Temperature 400 °C |
55100 psi @Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Ultimate | 380 MPa @Temperature 200 °C |
55100 psi @Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Ultimate | 380 MPa @Temperature 400 °C |
55100 psi @Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Ultimate | >= 380 MPa | >= 55100 psi | |
Misumi Z3234 Chromium Copper Excellent mechanical strength and abrasion resistance at high temperatures. Used in welding electrodes, seam welding wheels, switch gears, electrode holder jaws, cable connectors, current carrying a.. |
|||
Tensile Strength, Ultimate | 380 - 460 MPa | 55100 - 66700 psi | |
SSAB Tunnplat Docol® 260 BH High-strength Steel High-strength SteelComments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is ap.. |
|||
Tensile Strength, Ultimate | 380 - 460 MPa | 55100 - 66700 psi | |
SSAB Tunnplat Dogal 260 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Ultimate | >= 380 MPa | >= 55100 psi | |
SSAB Tunnplat Domex® 310YP Cold-forming Steel, HSLA Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®.. |
|||
Tensile Strength, Ultimate | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 380 MPa | >= 55100 psi | |
AK Steel ZINCGRIP® 275, Grade 40 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 380 MPa | >= 55100 psi | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, HSLAS, FORMABLE 40K / SAE J1392 040 XLK or 040 YLK Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 380 - 440 MPa | 55100 - 63800 psi | |
ArcelorMittal IF 260 High strength IF steel, Cold rolled Available in the following: uncoated (HC260Y), electroglavanized (HC260Y+ZE) and Extragal®/Galvannealed (HX260YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Tensile Strength, Ultimate | >= 380 MPa | >= 55100 psi | |
AK Steel ASTM A 1018, Grade 40 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 380 MPa | >= 55100 psi | |
AK Steel CL 2/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 380 MPa | >= 55100 psi | |
MetalTek MTEK ALLOY X Cast UNS N06002 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |