Polymer Property : Tensile Strength, Ultimate = 38.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.0 - 38.0 MPa
2610 - 5510 psi
Average value: 32.9 MPa Grade Count:59
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 16.0 - 38.0 MPa
2320 - 5510 psi
Average value: 27.4 MPa Grade Count:11
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum and ..