Polymer Property : Tensile Strength, Ultimate = 370 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 270 - 370 MPa
39200 - 53700 psi
SSAB Tunnplat Docol® DC02 (Fe P03) Deep-drawing Steel
Deep-drawing SteelComments: Docol - Cold Rolled Mild Steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.00 mm. Iron content is approximate - exact composition is not reported b..
Tensile Strength, Ultimate 320 - 370 MPa
46400 - 53700 psi
ArcelorMittal 14 High formability steel for drawing, Hot rolled
Available in the following: uncoated (DD14) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au..
Tensile Strength, Ultimate 270 - 370 MPa
39200 - 53700 psi
ArcelorMittal 55+AS Aluminized steel
Use: Very difficult drawing, 600°< T < 800°CInformation provided by ArcelorMittal