Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 249 MPa | 36100 psi | |
PCC-Advanced Forming Technology AlSiC-SD Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |