Polymer Property : Tensile Strength, Ultimate = 360 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.48 - 42.1 MPa
360 - 6100 psi
Average value: 25.2 MPa Grade Count:66
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Tensile Strength, Ultimate 2.48 MPa
360 psi
Momentive Performance Materials RTV1673LV One Component, Low Volatile Silicone Adhesive Sealant, Black
RTV1673LV one-component, ready-to-use adhesive sealants cures to a tough durable, resilient silicone rubber when exposed to atmospheric moisture at room temperature. Methyl alcohol and a small amoun..
Tensile Strength, Ultimate >= 2.48 MPa
>= 360 psi
ASTM D412
Multibase Multi-Flex® TPE A 4710 NAT
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Tensile Strength, Ultimate 2.48 MPa
360 psi
Dow Corning SE 738 SILICONE RTV
One-part, white, moisture cure RTV, non-flowing, general purpose, UL 94 HB.Information provided by Dow Corning
Tensile Strength, Ultimate 2.48 MPa
360 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 281-64MED Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..