Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 2.0 - 10 g/10 min
2.0 - 10 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 2.48 MPa
>= 360 psi
ASTM D412
Elongation at Break >= 525 %
>= 525 %
ASTM D412
Tear Strength >= 15.5 kN/m
>= 88.4 pli
ASTM D624