Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.7 MPa
5320 psi
Indium Corp. Indalloy® 9 Sn-Pb-In Solder Alloy
General purpose solder in 160° C range with good physical properties.Information provided by the manufacturer, Indium Corporation.