Polymer Property : Tensile Strength, Ultimate = 350 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.41 MPa
350 psi
Pyrotek Pyroboard™ S1000 Roller
Pyroboard™ S1000 is designed to be used throughout the preheat and cooling sections of the furnace.Information provided by Pyrotek.
Tensile Strength, Ultimate 2.41 MPa
350 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8201-67W228 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Tensile Strength, Ultimate 2.41 MPa
350 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Tensile Strength, Ultimate 2.41 MPa
350 psi
Typical properties based on film cast from toluene solution.; ASTM D412
Kraton® D1119 P (SIS) Linear Block Copolymer
Description: Kraton D1119 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: ..
Tensile Strength, Ultimate 2.41 MPa
350 psi
Dow Corning 832 MULTI-SURFACE ADHESIVE SEALANT
Neutral cure RTV sealant with very good adhesion to many substratesInformation provided by Dow Corning
Tensile Strength, Ultimate 2.41 MPa
350 psi
Dow Corning HM-2500 CLEAR ASSEMBLY SEALANT
A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning
Tensile Strength, Ultimate 2.41 MPa
350 psi
Dow Corning HS III BASE & 10:1 CLEAR CATALYST
High strength lower durometer silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items. HS III Base with HS III 10:1 Clear Catalyst is recommended f..
Tensile Strength, Ultimate 2.41 MPa
350 psi
Dow Corning HS IV BASE & 10:1 COLORED CATALYST
High strength lowest durometer silicone mold making rubber, suited for the production of print pads and for the detailed reproduction of fiines and art objects. HS IV Base with HS IV 10:1 Colored Ca..
Tensile Strength, Ultimate 2.41 MPa
350 psi
BCC Products MB 1100 Polyurethane Foam Modeling Board
MB 1100 is an Olive colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1100 is low density foam of approximately 10lbs/ft3 board. Easily cut using CNC machining equipment or ..
Tensile Strength, Ultimate 2.41 MPa
350 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..