ExxonMobil Santoprene® 8201-67W228 Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8201-67W228 Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Non-hygroscopic product, requires little to no drying before processing.Neutral, easy coloring formulation.Recommended for applications requiring excellent ozone resistance.Used in sealing applications.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 67

@Thickness 2.00 mm
67

@Thickness 0.0787 in
ISO 868
Tensile Strength at Break 6.07 MPa
880 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 2.41 MPa
350 psi
Across Flow; ASTM D412
Elongation at Break 460 %
460 %
Across Flow; ASTM D412
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets