Polymer Property : Tensile Strength, Ultimate = 35.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 35.9 MPa
5210 psi
ASTM Data
Styron Magnumâ„¢ 2610 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Ultimate 35.9 MPa
5210 psi
ASTM Data
Styron Magnumâ„¢ 9010 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Strength, Ultimate 35.9 MPa
5210 psi
ASTM Data
Styron Magnumâ„¢ FG960 ABS, High Impact
MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS ..
Tensile Strength, Ultimate 35.9 - 170 MPa
5200 - 24700 psi
Average value: 62.9 MPa Grade Count:84
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 35.9 MPa
5210 psi
ASTM D412
BASF Elastollan® M85A55 Polyester Type Polyurethane Elastomer
The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl..
Tensile Strength, Ultimate 35.9 MPa
5210 psi
ASTM Data
Styron Magnum™ 9100 MFD ABS
Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.