Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.38 MPa | 345 psi | |
Pyrotek Pyroboard™ S1150 Roller Pyroboard™ S1150 is designed for use in an enclosed furnace position where the atmosphere is consistent with strip temperature and does not exceed 2200° F.Information provided by Pyrotek. |