Material Notes:
Pyroboard™ S1150 is designed for use in an enclosed furnace position where the atmosphere is consistent with strip temperature and does not exceed 2200° F.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.753 g/cc
0.0272 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2.38 MPa
345 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1149 °C
2100 °F
Shrinkage 0.900 %

@Temperature 982 °C
0.900 %

@Temperature 1800 °F
Surface
1.00 %

@Temperature 982 °C
1.00 %

@Temperature 1800 °F
Thickness
2.30 %

@Temperature 1149 °C
2.30 %

@Temperature 2100 °F
Thickness
2.90 %

@Temperature 1149 °C
2.90 %

@Temperature 2100 °F
Surface
Users viewing this material also viewed the following: