Polymer Property : Tensile Strength, Ultimate = 335000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2310 MPa
335000 psi
hardness of 58 HRC
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel
Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are ..
Tensile Strength, Ultimate 2310 MPa
335000 psi
ATI Allvac® VascoMax® C-350 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
Data provided by Allvac.Applications: Missile components. Tooling. Spring wire for valve springs in high-performance internal combustion engines.