Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2310 MPa | 335000 psi | hardness of 58 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |
|||
Tensile Strength, Ultimate | 2310 MPa | 335000 psi | |
ATI Allvac® VascoMax® C-350 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age Data provided by Allvac.Applications: Missile components. Tooling. Spring wire for valve springs in high-performance internal combustion engines. |