Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 22.7 MPa | 3290 psi | Measured on extruded film, ASTM D638 |
3M Dyneon™ THV™ 500 Fluorothermoplastic
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Tensile Strength, Ultimate | 22.7 MPa | 3290 psi | ASTM D412 |
Dow Tyrin® CM2348P Formulation FormulationTyrin® CPE Elastomer |