Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Tyrin® CM2348P Formulation

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name Tyrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Tyrin® CM2348P Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationTyrin® CPE Elastomer
Physical Properties Metric English Comments
Mooney Viscosity >= 51

@Temperature 121 °C
>= 51

@Temperature 250 °F
ML 1 + 4; ASTM D1646
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
ASTM D2240
Tensile Strength, Ultimate 22.7 MPa
3290 psi
ASTM D412
Elongation at Break 320 %
320 %
ASTM D412
200% Modulus 0.0128 GPa
1.86 ksi
ASTM D412
Users viewing this material also viewed the following: