Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 221 MPa | 32000 psi | |
MTI ThermoStran® PA66-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 221 MPa | 32000 psi | ASTM D638 |
Applied Composites 175 Vinylester SMC Industry Application: TransportationProduct Application: Structural ExteriorDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation. |
|||
Tensile Strength, Ultimate | 221 MPa | 32000 psi | |
AIM 63Sn/Pb37 Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 221 MPa | 32000 psi | |
Parkway Products Thixomolded® AM60A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |