Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.38 MPa
490 psi
BCC Products DP-11-83 Urethane Adhesive-Slo
DP-11-83 is a low viscosity, quick setting, easy to use adhesive and/or casting material. This product was designed to bond together the MB1200 foam board to create desired dimensions in length, wid..
Tensile Strength, Ultimate 3.38 MPa
490 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Tensile Strength, Ultimate 3.38 MPa
490 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-80M300 Thermoplastic Elastomer  (discontinued **)
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good..
Tensile Strength, Ultimate 3.38 MPa
490 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..